Solid mixture of the batch of 10 classic requirements

by:Lisson     2020-11-11
1. Glass raw material granularity: 60 ~ 80 purpose > 85%, especially mineral raw materials;

2。 Glass raw material ingredient: stability, especially the control of feldspar and silica sands;

3。 Glass raw material moisture: < 8 ~ 10%, the focus is on silica sand, feldspar;

4。 Glass raw materials weighing accuracy: 1% ~ 1/3000;

5。 Feeding order: silica sand, soda ash and feldspar + auxiliary and small;

6. Mixing time: 3 ~ 5 minutes;

7。 Mixed uniformity: & ge; 96 ~ 98%;

8。 Water content: the batch of 5 ~ 7%;

9。 Broken glass: granularity & le; 50mm;

10. Blend to add the batch transportation blanking distance: & le; 1 meter gap.

more than 10 is a classic quality requirements, enterprises should achieve standardization control. According to & other; Two mixer & throughout; Theory, make uniform glass, solid mixture in the cold should account for 70%, and are more likely to do well, the key is understanding.
glass kiln in fact monitoring role: 1. Monitor the flame and melted; 2. Monitoring to the batch and the glass surface, such as bubble; 3. Monitor the fire-proof material absorption; 4. A hand-held within sight glass body can check the grid congestion and channel congestion; 5. To guide us to correct the role of the system.

a classic combustion gas bubbling electric melting glass furnace model